http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110560064-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7007ba2db892cc54b39fa0cebaf4e3c8 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-0033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-725 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-75 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-72 |
filingDate | 2019-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_817856ef94f82b4c22ce1ce9c58d4a86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_510324df719b504db512af2fc75238be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64ffac51886b2544fd5eb88abc6e9972 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89a0f312c1777b7923948eab685bc56f |
publicationDate | 2019-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110560064-A |
titleOfInvention | A kind of preparation method and application of magnetic carbon ball supported tricobalt tetroxide catalyst |
abstract | The invention discloses a preparation method and application of a magnetic carbon ball-supported tricobalt tetroxide catalyst. The preparation method of the magnetic carbon ball-supported tricobalt tetroxide catalyst comprises: adding an iron salt solution to a carbon-containing compound solution, stirring to form a mixed solution; The liquid is heated to 80-160°C for hydrothermal reaction for 6-20h, then solid-liquid separation and collection of solid products, washing and drying of the solid products to obtain magnetic carbon spheres; adding the magnetic carbon spheres to the cobalt salt solution After dispersing evenly, adding ammonia aqueous solution, stirring and mixing, heating to 120-180 ° C for hydrothermal reaction for 8-20 hours, then solid-liquid separation and collecting solid products, washing and drying the solid products to obtain magnetic carbon balls supported Cobalt tetroxide catalyst. The magnetic carbon ball-supported tricobalt tetroxide catalyst prepared by the invention has high catalytic performance when catalyzing and activating persulfate to degrade aniline wastewater, and is easy to recover. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113996174-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114558559-A |
priorityDate | 2019-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.