Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2383-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2483-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2483-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2383-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-0504 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01C10-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01L1-205 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01L1-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 |
filingDate |
2018-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2021-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2021-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-110546193-B |
titleOfInvention |
Pressure-sensitive elastomer porous body |
abstract |
A pressure-sensitive elastomer porous body, which is a cured product of an elastomer emulsion obtained through an emulsion composition having a liquid rubber material that is cured to form an elastomer as a continuous phase, wherein relative to the above The total amount of the emulsion composition contains a conductive agent in an amount of 2.7% by weight or more and 3.5% by weight or less, and the resistance value (Ω) increases as the compression ratio C (%) increases. |