http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110423036-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_40c3a24acafc39846109b5a181a69878 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-65 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-65 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-08 |
filingDate | 2019-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd46749119f9c50f2284295e1ace6ba7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c040bf444499ffead07e61343ca69b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ce35d3da70e27a853f1ddfdff18cc2d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d5bf06bf7bd5187629aa9132dc6d5f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5895894dd9ba0dbd9cd2f11dd012b84c |
publicationDate | 2019-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110423036-A |
titleOfInvention | A long-lasting waterproof wall waterproofing agent and its processing technology |
abstract | The invention discloses a long-acting waterproof wall waterproofing agent, which comprises stearic acid, sodium carbonate, potassium hydroxide, ferric chloride, calcium chloride, ammonia water and water; its components are calculated by weight percentage: stearin Acid 3%-5%, Sodium Carbonate 0.1%-0.3%, Potassium Hydroxide 0.7%-0.9%, Ferric Chloride 25%-27%, Calcium Chloride 22%-24%, Ammonia 2%-4% and Water 42%‑44%; the processing technology includes raw material preparation, raw material melting, raw material primary mixing, raw material secondary mixing, and sieving to obtain the finished filtrate; the wall waterproofing agent of the present invention is added with stearic acid, which has good waterproof performance and long waterproof life , Low process difficulty and low cost; adding sodium carbonate is an alkali metal compound, which has a plasticizing effect, can reduce the water-cement ratio, cut and reduce seepage channels, increase the compactness of the mortar, and make the mortar waterproof; add ferric chloride , with iron oxide scale and iron powder as the main raw materials, ferric chloride waterproofing agent has the effect of strengthening and early strength, and can continuously improve the compressive strength of concrete and have a relatively high impermeability in the early stage. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113845329-A |
priorityDate | 2019-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.