Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_70b5d1f743f93e4b8753d6e39c771bad |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-745 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-745 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 |
filingDate |
2019-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_713b5d51e8c5f7404ff6d8e9f32b8da9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa5e0d88a1d7ec2380bd2281beaf1f3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_deceda1eafccc9cb3a69965bab5bd340 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85b4100051d331b4f073474be71a7baf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a1df41babf122675b47162cfbb7b32b |
publicationDate |
2019-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-110394178-A |
titleOfInvention |
Nano-iron trioxide/nano-titanium dioxide composite photocatalyst and preparation method |
abstract |
The invention discloses a nano-iron trioxide/nano-titanium dioxide composite photocatalyst and a preparation method thereof, belonging to the field of photocatalytic environment restoration. The preparation method has the following steps: 1. Dissolving 0.2g-1.80g of ferric nitrate nonahydrate in distilled water, then adding 0.10g-0.80g of citric acid and a certain amount of sodium chloride to the solution of ferric nitrate nonahydrate; 2. Stir to obtain a uniform solution; 3. Then add commercially available P25 titanium dioxide powder to the above solution, and ultrasonically disperse to prepare a suspension; 4. The above suspension is transferred to a tube furnace for combustion, and the reaction kettle is naturally cooled after the reaction is completed Repeated washing after reaching room temperature; 5. After washing, the samples were placed in a vacuum drying oven to dry at a temperature of 60°C and a time of 2h. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111871407-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111604052-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111205426-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111227427-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111205426-B |
priorityDate |
2019-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |