http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110330834-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b7b034a5e1f490953f1e7df9f47e9470 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-101 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-102 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-101 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-03 |
filingDate | 2019-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3ada64f74f754a47089ab4ac0e842f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e59da6c386cadaea5797f6c9c5e7738 |
publicationDate | 2019-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110330834-A |
titleOfInvention | A kind of UV cured printing ink and preparation method thereof for glass baseplate |
abstract | The invention discloses a kind of UV cured printing inks for glass baseplate, it is characterised in that it includes each raw material of following parts by weight is made: propylene acyloxy methyl modified 40-50 parts of epoxy-terminated polyurethane double-end amino silicone oil condensation polymer, 10-15 parts of ultra-branched polyurethane acrylate, super-branched polyimide 10-20 parts acrylate modified, 3-6 parts of phenyl vinyl sulfide, 3-5 parts of N- vinylpiperidone, 1-3 parts of activated silica, 0.1-0.3 parts of coupling agent, 3-6 parts of photoinitiator.The invention also discloses the preparation methods of the UV cured printing ink for glass baseplate.UV cured printing ink disclosed by the invention for glass baseplate has good adhesive force and high fastness, and good weatherability, high-efficiency environment friendly, excellent combination property, covering power is good, water-fast, heat resistance is good, and it can directly be printed upon on glass, and rate of drying is fast. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110845202-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112721357-A |
priorityDate | 2019-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.