http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110308501-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-06 |
filingDate | 2019-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2022-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2022-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110308501-B |
titleOfInvention | Strong laser film and preparation method and application thereof |
abstract | The invention discloses a strong laser film, a preparation method and application thereof, and belongs to the technical field of strong laser materials. The ultraviolet curing silicone film can realize high transmission at fundamental frequency and frequency doubling positions and can reduce the transmissivity at the frequency doubling positions by controlling the content of the ultraviolet initiator and absorbing the frequency tripling laser in an ultraviolet band while realizing film curing. The film provided by the invention has high transmissivity at fundamental frequency and frequency doubling wavelength, and both can be higher than 99%. The film provided by the invention has high triple frequency absorption cutoff capacity, and the transmissivity of the film is lower than 90%. |
priorityDate | 2019-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links