http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110305553-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1668 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-14 |
filingDate | 2019-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110305553-B |
titleOfInvention | A kind of geopolymer-based antibacterial coating and preparation method and application thereof |
abstract | The invention discloses a geopolymer-based antibacterial coating and a preparation method and application thereof. The coating is composed of 15-50 parts by weight of component A, 20-70 parts by weight of component B and 10-50 parts by weight of component C; the said component A is composed of 40-80 parts by weight of geopolymer gel base material and 20-60 parts by weight of pigments and fillers; the B component is composed of 40-85 parts by weight of alkali activator, 0-15 parts by weight of curing regulator, 0-6 parts by weight of rheology modifier and 12-45 parts by weight of The C component is composed of 70-100 parts by weight of antibacterial telomer and 0-30 parts by weight of silane modifier. The coating of the invention has zero VOCs, is green, environmentally friendly, healthy, and has excellent corrosion resistance. More importantly, the coating can effectively inhibit the growth and reproduction of microorganisms, has the characteristics of high efficiency and antifouling, and is suitable for cultural relics, buildings, and freshwater aquaculture. Waterproof, anti-corrosion, antibacterial and anti-biofouling for steel structures and concrete surfaces. |
priorityDate | 2019-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 150.