http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110272683-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 |
filingDate | 2019-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110272683-B |
titleOfInvention | Wear-resistant super-hydrophobic coating, preparation method thereof and method for preparing coating |
abstract | The invention discloses a wear-resistant super-hydrophobic coating, a preparation method thereof and a method for preparing a coating, wherein the method is simple, convenient and universal, can be used for large-area preparation, and solves the problems that the existing super-hydrophobic coating is difficult to produce on a large scale, the mechanical property can not meet the actual requirement, the durability is poor and the like. The coating comprises the following components in percentage by mass: trifunctional nano-silicon spheres: 8.4-23.2%; alkyl siloxane: 4.8-9.5%; hydrogen-containing silicone oil: 1.9-4.6%; deionized water: 3.1-9.4%; alcohol solvent: 59.7-75.6%; acid catalyst: 0.15-0.22%; platinum catalyst: 0.2 to 0.4 percent. |