http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110148742-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 |
filingDate | 2019-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110148742-B |
titleOfInvention | Preparation process of iron carbide/carbon ultrathin nano-sheet composite electrode material for lithium ion battery |
abstract | The invention discloses a preparation process of an iron carbide/carbon ultrathin nano-sheet composite electrode material for a lithium ion battery, which comprises the steps of cleaning biomass waste with alcohol, then carrying out vacuum drying, crushing into powder, and sieving to obtain powder A; adding an acid solution into the powder A, and stirring to obtain a mixture B; transferring the mixture B into a hydrothermal induction kettle, adding carbon cloth as an induction source, transferring the hydrothermal induction kettle into hydrothermal induction heating equipment for reaction, cooling to room temperature, taking out the carbon cloth, scraping the obtained product, washing with deionized water and ethanol, performing suction filtration, and drying to obtain powder C; preparing an iron source solution, adding the powdery C into the iron source solution, and heating and stirring to obtain D; calcining D in a protective atmosphere, cooling to room temperature, washing, filtering and drying the obtained product by deionized water and ethanol to obtain Fe 3 C/C ultrathin nanometer sheet-shaped composite electrode material. |
priorityDate | 2019-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |