http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110099947-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-1046 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 |
filingDate | 2017-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110099947-B |
titleOfInvention | Method for preparing polyetherimide and polyetherimide prepared by the method |
abstract | A method for preparing an isolated polyetherimide composition, comprising combining a synthesized polyetherimide containing a unit of formula (I) and a melt-stabilizing amount of tri(C 8-30 acyl) glycerides, formula The anhydride of (II) or a combination comprising at least one of the foregoing to provide a mixture; and isolating the polyetherimide composition from the mixture to provide an isolated polyetherimide composition having within 30 minutes Complex viscosity change measured at 390°C, shear rate 6.28 rad/s, strain = 5%, and nitrogen is +15% to -20%, preferably from +10% to -20%, more preferably from +5 % to ‑20%. |