http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110041806-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_63b03db9fef33af7af219f14bb7901cf |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-0806 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D191-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D189-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D105-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D101-28 |
filingDate | 2019-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef3a497a57f52c718cd089318208b271 |
publicationDate | 2019-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-110041806-A |
titleOfInvention | A kind of environmental protection moisture-proof coating for wall and preparation method thereof |
abstract | The invention discloses an environment-friendly moisture-proof coating for walls and a preparation method thereof. 1) Add soybean protein isolate to a solvent, stir and mix evenly, and then add titanium dioxide to obtain material A; 2) Add biological enzymes to the solvent, stir evenly, To obtain material B, 3) Add the remaining solvent, film-forming substance, and film-forming aid to the stirring tank, heat, stir and disperse evenly; 4) Add filler, defoamer, wetting agent and antibacterial agent, stir and disperse evenly ;5) Use the air compressor to spray the melted microcrystalline paraffin into the stirring tank. After adding the microcrystalline paraffin, add material A into the stirring tank, continue stirring evenly and then cool to room temperature; 6) Stop heating and wait for stirring After the material in the tank is cooled to room temperature, material B is added to the stirring tank, stirred and mixed, allowed to stand, and discharged to obtain the environmental protection moisture-proof coating. The coating of the invention has the functions of removing indoor formaldehyde and purifying the air, has superior moisture-proof ability, and can effectively maintain the dryness of the wall. |
priorityDate | 2019-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links