http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109853023-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cc4e13141d402ceb885f368dfa042348 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-36 |
filingDate | 2019-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01c63932f20d5ae8d43e00757bd5846d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f00525fa45ba53a924a9e2f7c2879920 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0c53b1ef9bda0c560aa58c2ca2a7536 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dccc3dbca0d7e6c12fa0e5c70611b20d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4eb1f21c2dce342bb5a57c9cc01d0f64 |
publicationDate | 2019-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109853023-A |
titleOfInvention | A kind of zinc-based anti-corrosion electrolytic phosphating solution and preparation method thereof |
abstract | The invention discloses a zinc-based anticorrosion electrolytic phosphating solution and a preparation method thereof. In parts by mass, the raw material formula components of the solution include: Zn 2+ 1-10 parts; PO 4 3-10-50 parts; functionalized 0.01-1 part of graphene oxide; 5-15 parts of pH regulator; 1000 parts of water. Preparation of functionalized graphene oxide: disperse graphene oxide in absolute ethanol, react with silane coupling agent at temperature and reflux, after suction filtration and washing, disperse in deionized water to obtain a dispersion; the obtained dispersion, cationic monomer, The initiator and deionized water are put into the reaction kettle, the temperature is raised to react, and after suction filtration and washing, it will be dispersed in deionized water to obtain the product. The electrolytic phosphating solution prepared by the invention can well solve the problem of the dispersibility of graphene oxide in the electrolytic phosphating solution without using surfactants and stabilizers, and the preparation process of the electrolytic phosphating solution is non-toxic and harmless, and the process Simple, convenient and controllable, and conducive to industrialization. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113045962-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113045962-A |
priorityDate | 2019-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 80.