titleOfInvention | Metal roof acrylic acid high-elasticity waterproof coating and preparation method thereof |
abstract | The invention relates to a building waterproof coating, and provides a metal roof acrylic acid high-elasticity waterproof coating, which comprises a component A and a component B; the component A at least comprises the following raw materials: solvents, dispersants, defoamers, fillers, chloride salts, fumed silica, pigments; the component B at least comprises the following raw materials: the coating comprises a covering emulsion, a defoaming agent, a film-forming auxiliary agent, a bactericide, a weakly alkaline reagent, small molecular alcohol and a thickening agent. |