classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-14 |
filingDate | 2019-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109825231-B |
titleOfInvention | Flame-retardant ultraviolet-resistant epoxy encapsulating adhesive and preparation method thereof |
abstract | The invention belongs to the technical field of high polymer materials, and particularly relates to a flame-retardant ultraviolet-resistant epoxy encapsulating adhesive and a preparation method thereof, wherein the flame-retardant ultraviolet-resistant epoxy encapsulating adhesive comprises a component A and a component B, wherein the weight ratio of the component A to the component B is 100: 20-45; the component A comprises: 50-80 parts of modified epoxy resin, 15-20 parts of flame-retardant light stabilizer, 20-30 parts of diluent, 5-15 parts of filler, 3-8 parts of thixotropic agent, 10101-3 parts of antioxidant and 0.5-1 part of defoaming agent; and B component: 45-60 parts of curing agent, 10-20 parts of accelerator and 0.5-1 part of defoaming agent. The flame-retardant ultraviolet-resistant epoxy encapsulating adhesive and the preparation method thereof have the advantages of high bonding strength, body strength and hardness, high mechanical strength, low shrinkage, excellent electrical insulation performance, good chemical stability, excellent flame retardance and ultraviolet resistance; the preparation method is simple, easy to operate, wide in raw material source, low in cost, environment-friendly and pollution-free. |