http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109797354-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2136ed4fefdf5dc70807b7f61979c2d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22F1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D1-26 |
filingDate | 2017-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86527adc279aa246b05158c005d4a6e8 |
publicationDate | 2019-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109797354-A |
titleOfInvention | A kind of copper wire annealing liquid |
abstract | The present invention relates to copper wire manufacture fields, in particular to a kind of copper wire annealing liquid, according to parts by weight, including following component: 10 ~ 20 parts of base oil, 15 ~ 25 parts of lubricant, 20 ~ 30 parts of palm oil grease, 10 ~ 20 parts of ricinolein, 1 ~ 5 part of metal antioxidant, remaining be distilled water.Lower production costs of the invention, proportion rationally, improve the plasticity and flexibility of copper wire, and intensity is increased to 300 ~ 400mpa by original 240mpa, and elongation percentage improves 8% ~ 10%, and anti-oxidant degree was increased to 35 days or so by original 10 days. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115433891-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110860569-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110860569-B |
priorityDate | 2017-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 18.