titleOfInvention | Preparation method of aluminum silicon carbide material and prepared aluminum silicon carbide material |
abstract | The invention discloses a preparation method of an aluminum silicon carbide material and the prepared aluminum silicon carbide material. According to the preparation method of the aluminum silicon carbide material, silicon carbide soaked by aluminum is mixed with the aluminum alloy melt, so that silicon carbide particles are fully wetted by the aluminum before being mixed with the aluminum alloy melt, and then the silicon carbide material soaked by the aluminum is diluted by the aluminum alloy melt through a stirring casting method, so that the aluminum silicon carbide material is prepared. The preparation method is simple and convenient, and is easy to operate and control the reaction process. Because the silicon carbide surface wraps up aluminium for silicon carbide particle is fully moistened, just fuse with the aluminium alloy melt more easily when adding it in the aluminium alloy melt again, can dissolve more carborundum in the aluminium alloy melt of the same volume promptly, improves carborundum content in the aluminium carborundum material. |