http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109735025-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-16 |
filingDate | 2019-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109735025-B |
titleOfInvention | Antistatic PVC (polyvinyl chloride) plate material as well as preparation method and application thereof |
abstract | The invention relates to an antistatic PVC sheet material, a preparation method and application thereof, wherein the PVC sheet material comprises the following preparation raw materials in parts by weight: 80-90 parts of polyvinyl chloride resin, 90-100 parts of filler, 6-10 parts of composite antistatic agent, 40-50 parts of plasticizer, 1.5-3.5 parts of auxiliary plasticizer, 3-4.5 parts of stabilizer, 1-2 parts of processing aid and 1-2 parts of lubricant; the composite antistatic agent comprises calcium chloride and bis (2-hydroxyethyl) amine. The preparation method comprises the following steps: and (2) adding the preparation raw materials of the antistatic PVC plate material into a mixer according to the parts by weight, mixing, then carrying out open milling in an open mill, and finally pressing into tablets in a press. The antistatic PVC sheet material has reasonable component formula, obvious antistatic effect, stable and durable antistatic performance and low dependence on environmental humidity. |
priorityDate | 2019-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 36.