http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109659500-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-027 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0566 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-134 |
filingDate | 2018-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109659500-B |
titleOfInvention | Lithium sheet for reducing interfacial impedance of solid electrolyte/lithium cathode, preparation method and application |
abstract | The invention discloses a preparation method of a lithium sheet for reducing the interfacial impedance of a solid electrolyte/lithium cathode, which comprises the following steps: s1, respectively weighing a small molecular solid solvent and a lithium salt for later use; wherein the mass ratio of the micromolecular solid solvent to the lithium salt is 70-95: 5-30; s2, dissolving the micromolecule solid solvent weighed in the S1 in an organic solvent, stirring at room temperature for 24 hours to obtain a mixed solution, and then adding the lithium salt weighed in the S1 into the mixed solution to dissolve the lithium salt to obtain a micromolecule electrolyte solution; and S3, coating the micromolecule electrolyte solution obtained in the S2 on the surface of a lithium sheet, and then drying in vacuum at a certain temperature to obtain the lithium sheet for reducing the interface impedance of the solid electrolyte/lithium cathode. The invention also discloses the application of the lithium sheet in the all-solid-state lithium battery, and the lithium sheet can reduce the interface impedance between the solid electrolyte and the lithium sheet and improve the cycle performance of the battery in the charge and discharge processes of the all-solid-state lithium battery. |