http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109637840-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d1a291fb43e0fc4fbd3e1a262d96750d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-86 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-86 |
filingDate | 2019-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_863e57da133201ca68d6346672f3e50f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c2e9bc9993afd4325f9f200005aaea4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e656fa94c1eb5af49246f7982870f29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a1008283ed1fd9e2c3c05d0a186012dc |
publicationDate | 2019-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109637840-A |
titleOfInvention | A kind of NiFe2O4/carbon nanosheet composite material and preparation method thereof |
abstract | The invention relates to a NiFe 2 O 4 /carbon nano-sheet composite material and a preparation method thereof, belonging to the technical field of carbon composite materials. The preparation method of the present invention comprises the following steps: performing TEMPO catalytic oxidation on chitin raw materials and cellulose raw materials, respectively, to obtain a chitin nanofiber suspension and a cellulose nanofiber suspension; mixing the two evenly to obtain a composite suspension; adjusting The pH value of the composite suspension is 12; add an inorganic salt solution and mix evenly; hydrothermally react at 180-200 ° C for 20-22 h to obtain a composite hydrogel; immerse in water until the composite hydrogel reaches neutrality to obtain neutrality composite hydrogel; freeze and dry to obtain composite aerogel; in an inert atmosphere, keep the temperature at 600°C-900°C for 3 hours, and then obtain. The NiFe 2 O 4 /carbon nano-sheet composite material prepared by the method of the invention has uniform particle distribution and uniform size. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110211811-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110280271-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110280271-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115282330-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112844255-A |
priorityDate | 2019-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.