http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109486063-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-202 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-443 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 |
filingDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109486063-B |
titleOfInvention | Polyurethane modified polyvinyl chloride cable material resistant to scratching and abrasion and preparation method thereof |
abstract | The invention discloses a polyurethane modified polyvinyl chloride scraping and abrasion resistant cable material and a preparation method thereof, wherein the cable material comprises the following components in parts by weight: 30-40 parts of polyvinyl chloride, 10-20 parts of polyurethane prepolymer, 0.02-0.12 part of cross-linking agent, 15-20 parts of plasticizer, 15-20 parts of filler, 7-13 parts of modifying assistant, 3-5 parts of stabilizer and 0.4-1 part of lubricant; the preparation method comprises the following steps: adding other raw materials except the polyurethane prepolymer into a high-speed mixer for mixing, then adding the mixture and the polyurethane prepolymer into an internal mixer for banburying, and finally granulating to obtain the polyurethane elastomer. The cable material can effectively solve the problems of poor scratch and abrasion resistance and easy abrasion existing in the conventional cable material. |
priorityDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.