http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109455972-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 |
filingDate | 2018-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109455972-B |
titleOfInvention | Preparation method of aluminum silicate accelerator |
abstract | The invention relates to a preparation method of an aluminum silicate accelerator, which comprises the following steps: adding soluble silicate into a solution containing a dispersing agent, preferably dropwise, to form a mixed solution; adding soluble aluminum salt into the prepared mixed solution, preferably dropwise, so as to react with the soluble silicate to generate a suspension containing aluminum silicate; and adding a setting time regulator into the aluminum silicate-containing suspension to prepare the aluminum silicate accelerator. The preparation process is simple, the process is economic and environment-friendly, and the prepared aluminum silicate accelerator can obviously shorten the quick setting time and the final setting time. |