http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109331544-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d40285e27f4ed83b8728b0d477404958 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2239-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D39-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F226-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D39-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F226-10 |
filingDate | 2018-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd736f358f49fcfba9090f7985f316e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91b62af02aa9d75dcd8e86336d55b286 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08a93c866f8619551896279f45624531 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ceed06b20a7d80a8fee84a060b2499ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_116163d1b15fb3cb78223d85b8eaffc9 |
publicationDate | 2019-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109331544-A |
titleOfInvention | A kind of durable hydrophilic modified polyethylene filter element and preparation method thereof |
abstract | The invention discloses a durable hydrophilic modified polyethylene filter element and a preparation method thereof. The method comprises the following steps: dissolving a hydrophilic monomer, a crosslinking agent and an initiator in a solvent, and mixing them uniformly to obtain a modified polyethylene filter element. solution; the polyethylene powder is wetted with the modified solution and then pressed into the filter element mold, and the hydrophilic monomer chemical cross-linking reaction is carried out in the filter element mold, and then sintered to obtain a durable hydrophilic modified polyethylene powder. vinyl filter products. In the present invention, the cross-linked polyethylene powder particles are coated with a hydrophilic monomer, and the sintered polyethylene filter element is prepared to obtain a durable hydrophilized polyethylene filter element. The polyethylene filter element prepared by the method is chemically cross-linked due to the coating of the hydrophilic monomer on the surface of the polyethylene powder particles, so the hydrophilicity can remain unchanged after long-term operation, thereby significantly reducing the operating pressure and improving the pollution degree. Improve operational efficiency. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112316491-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112726016-A |
priorityDate | 2018-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.