Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2211-1029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2211-1088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-281 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F230-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F230-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-28 |
filingDate |
2017-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2020-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2020-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-109293823-B |
titleOfInvention |
Process for preparing solid red-to-yellow conversion copolymer system |
abstract |
The invention discloses a preparation method of a solid red-to-yellow up-conversion copolymer system, which takes α -hydroxyethyl methacrylate (HEMA) and 3- (methacryloyloxy) propyl trimethoxy silane (TMSPMA) as monomers, and evenly coats a sensitizer (sandwich type palladium phthalocyanine) and a luminescent agent (rhodamine series compound) in a certain ratio by in-situ polymerization under the initiation of azoisobutyronitrile to obtain the solid red-to-yellow up-conversion silicon copolymer, thereby solving the problem that deoxidization is needed in a solution state, more importantly solving the bottleneck problem that the current solid polymer has low up-conversion efficiency under the excitation of a 655nm semiconductor laser (laser power density is 1W × cm) ‑2 ) Up-conversion efficiency (F) of the solid copolymer obtained by the present invention UC ) Up to 12.75%; and in the air atmosphere, the conversion efficiency value on the solid can be kept more than 4 days to be almost not attenuated; has application value in the field of solar energy utilization. |
priorityDate |
2017-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |