http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109281205-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06B23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06P3-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06B3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06P1-0032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06P1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06B15-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06B3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06P3-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06P1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06P1-00 |
filingDate | 2018-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109281205-B |
titleOfInvention | Dyeing and finishing process of terylene hole four-side elastic cloth |
abstract | The invention relates to a dyeing and finishing process of terylene hole four-side elastic cloth, which specifically comprises the following steps: unwinding, preshrinking, cold piling, desizing, blank fixing, desizing in a cylinder, dyeing in the cylinder, dehydrating, scutching, shaping, winding and packaging, wherein the preshrinking step comprises the steps of pre-wetting by using over-warm water and then loading on a drying cylinder, the speed of the drying cylinder is 65-70 m/min, and the pressure of a roller is 1.5-2.0 kg/cm 2 And the temperature of each drying cylinder is regulated and controlled. The invention makes the shrinking width of the fabric uniform through preshrinking and avoids the crease abnormity caused by high temperature shock shrinkage, the fabric is fully shrunk at a certain temperature through cold heaping so as to enable the fiber to be more compact, bulkier and plump, the fabric is uniformly shrunk and shaped in advance at a high temperature through blank shaping, and simultaneously the molecular structure of the fiber is rearranged so as to be beneficial to dyeing. |
priorityDate | 2018-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.