http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109280450-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2244 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F283-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F238-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-08 |
filingDate | 2018-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109280450-B |
titleOfInvention | Epoxy acrylic resin flame-retardant coating and preparation method thereof |
abstract | The invention discloses an epoxy acrylic resin flame-retardant coating and a preparation method thereof, wherein the coating comprises the following raw materials in percentage by weight: 20-40 parts of epoxy acrylate prepolymer, 15-40 parts of flame retardant, 0.5-1.5 parts of initiator, 4-10 parts of pigment, 1.5-3.5 parts of dispersant, 4-10 parts of inorganic filler, 2-5 parts of defoaming agent, 2-6 parts of film-forming assistant and 5-30 parts of solvent. According to the invention, the reactive flame retardant is added into the matrix resin, and the flame retardant and the acrylate prepolymer form a completely compatible whole, so that the prepared flame-retardant coating not only has an excellent and durable flame-retardant effect, but also has excellent physical and mechanical properties, water resistance, chemical corrosion resistance and higher bonding strength. |
priorityDate | 2018-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |