abstract |
The invention discloses a metal paint for quick-drying stainless steel sheet, which has the following raw materials according to the weight: 12-18 parts of hydrogenated butyl cyanide rubber, 8-12 parts of linseed oil, 1.2-1.5 parts of copper powder, and dodecane 0.2-0.7 parts of base glycol amide, 1.5-2.3 parts of polyether siloxane copolymer, 7-11 parts of talc, 1.2-1.4 parts of rutile type titanium dioxide, 5-15 parts of polyurethane modified epoxy resin, methyl group 0.3 to 0.7 parts of acryloxysilane, 3.7 to 4.2 parts of mica powder, 8 to 15 parts of ethyl acetate, 15 to 20 parts of fine asbestos, 4 to 9 parts of urea-formaldehyde resin, and 0.4 to 0.8 of hydroxyethyl cellulose. The fraction is 0.2 to 0.8 parts of triphenyl phosphite, 5 to 10 parts of an acetylene glycol antifoaming agent, and 0.2 to 0.7 parts of butyl acetate. The paint of the invention has the advantages of environmental protection, non-toxicity, convenient use and low cost. |