http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109265969-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d8a5f14d0ee37db1c5e49b1b580b83b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-387 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 |
filingDate | 2018-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_313f01036c2040a2a3b1cb529c726a00 |
publicationDate | 2019-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109265969-A |
titleOfInvention | Nitrile rubber polyurethane composite material and preparation method thereof |
abstract | The invention relates to a nitrile rubber polyurethane composite material and a preparation method thereof, and belongs to the technical field of composite materials. Solved the technical problem of how to further improve the wear resistance of polyurethane. The composite material of the present invention is grafted with 100 parts by weight of polyurethane, 20-30 parts by weight of nitrile rubber, 2-5 parts by weight of chlorinated polyethylene, 1-3 parts by weight of sodium stearate, and 1.5-2.5 parts by weight of maleic anhydride. Polypropylene, 2 - 4 parts by weight of paraffin, 2.5 - 3.5 parts by weight of flame retardant, 1 - 2 parts by weight of antioxidant, 0.2 - 0.3 parts by weight of sodium lauryl sulfate, 1 - 2 parts by weight of polydimethylsiloxane Oxane, 1-2 parts by weight of heat stabilizer, 4-6 parts by weight of carbodiimide, 0.5-1 part by weight of castor oil, 1-3 parts by weight of nano silicon nitride powder, 0.5-0.8 parts by weight of wollastonite powder And 1 - 1.5 parts by weight of potassium acetate. The composite material has high wear resistance, good mechanical properties, good impact resistance and good heat resistance. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112831175-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112831175-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109942925-A |
priorityDate | 2018-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 77.