abstract |
The present invention provides a fluoropolymer and a process for the preparation thereof. The fluoropolymer has the following structural formula: Where n is 1 to 300. It can be seen from the above structural formula that the content of the aromatic ring in the fluoropolymer of the present application is substantially saturated, and therefore, the high temperature resistance of the fluoropolymer can be ensured; and the olefin group is not contained in the structural formula, and The content of fluorine element also reaches the maximum value of the chemically acceptable structure, so that the surface energy of the fluoropolymer is low, exhibiting very good hydrophobic oleophobic property, thereby reducing its adhesion. |