http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109232894-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-06 |
filingDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109232894-B |
titleOfInvention | Methoxy-terminated methylphenyl polysiloxane resin, organic silicon coating adhesive, preparation method and application |
abstract | The invention relates to methoxy-terminated methyl phenyl polysiloxane resin, an organic silicon coating adhesive, a preparation method and application thereof, wherein siloxane monomers for preparing the methoxy-terminated methyl phenyl polysiloxane resin comprise the following components in parts by weight: 19-30 parts of diphenyl dimethoxysilane, 20-30 parts of dimethyl dimethoxysilane and 40-60 parts of methyl trimethoxysilane; the mass content of phenyl in the methoxy-terminated methylphenyl polysiloxane resin is 23-25%. The methoxy-terminated methyl phenyl polysiloxane resin is terminated by methoxy groups and has a proper content of phenyl groups, so that the refractive index of the methoxy-terminated methyl phenyl polysiloxane resin is very close to that of fumed silica and the methoxy-terminated methyl phenyl polysiloxane resin has proper viscosity. The polysiloxane resin is adopted to replace a base material in the traditional organic coating adhesive, and the fumed silica is added as a reinforcing agent, so that the mechanical properties such as hardness, tensile strength and the like, the adhesive property and the air tightness can be obviously improved on the basis of ensuring high transparency. |
priorityDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |