http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109109142-B

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3217
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-9653
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3227
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3225
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6567
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6562
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-622
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B7-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62605
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B7-42
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-645
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B11-243
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B11-24
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-626
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B7-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-645
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B7-42
filingDate 2018-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2020-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2020-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-109109142-B
titleOfInvention Method for hot-press sintering of AlON by utilizing graphite mold for hot-press sintering of AlON transparent ceramic
abstract A method for hot-pressing and sintering AlON by using a graphite mold for hot-pressing and sintering AlON transparent ceramic comprises a mold main body and a base, wherein the mold main body comprises a central cavity, the height of the whole cavity is 130mm, and the cavity of the mold is provided with a taper; the upper part and the lower part of the die main body are respectively provided with a step part, and the upper part of the base is provided with a boss part corresponding to the step part. The graphite gasket is arranged in the cavity to isolate powder, the thickness of the graphite gasket is 4mm, the inner wall of the cavity of the die is provided with exhaust holes which are circular or cross-shaped, and the number of the exhaust holes is gradually reduced in the height direction of the die from bottom to top. The density of the sintered product is improved, and the finished product rate, the mechanical property, the optical property and the like are improved.
priorityDate 2018-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID947
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID702
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451818717
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419538410
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID9989226
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419556970

Total number of triples: 36.