http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109096840-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ae553cdba91e972d37e7b26ddbe5634 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 |
filingDate | 2018-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_044c2bae4cebe94f091bc2bf6f7148c2 |
publicationDate | 2018-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109096840-A |
titleOfInvention | A kind of mould proof water paint of non-toxic anticorrosion and its methods for making and using same |
abstract | The invention discloses a kind of mould proof water paint of non-toxic anticorrosion and its methods for making and using sames, including following composition by weight: 100-130 parts of water-base resin, 2 parts of mould inhibitor, 5-10 parts of preservative, 2 parts of organosilicon levelling agent, 2-8 parts of surfactant, 30-40 parts of water, 20-30 parts of pigment, pigment include following composition by weight: 20-30 parts of lead chromate yellow, 10-15 parts of iron oxide yellow, 18-25 parts of lead silico-chromate, 10-15 parts of strontium calcium yellow, 8-10 parts of transparent yellow, 2-10 parts of benzidine yellow, 1-8 parts of Chinese sand yellow, 5-7 parts of lemon yellow;The following steps are included: S1: weigh proportion, S2: blend the first mixture, S3: blending the second mixture, S4: proportion surfactant obtains finished product;The mould proof water paint of non-toxic anticorrosion is applied to inner wall of building decorative paint and exterior wall waterproofing coating.Application field is relatively broad while simple production process of the present invention, greatly reduces production cost, while production and use process will not generate noxious material, additionally it is possible to play the role of anticorrosive mildewproof. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110256916-A |
priorityDate | 2018-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.