http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109053216-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B38-0615 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-05 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-06 |
filingDate | 2018-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-109053216-B |
titleOfInvention | Block material with wetting anisotropy and preparation method thereof |
abstract | The invention discloses a bulk material with wetting anisotropy. The block body material consists of a plurality of carbon tubes, and the tube walls of the carbon tubes are mutually gathered to form a three-dimensional structure; the water droplets have hydrophobicity on the tube wall side of the carbon tube and hydrophilicity on the end face side of the carbon tube. The method comprises the steps of soaking the template in an ethanol solution of phenolic resin, heating to volatilize ethanol, heating to solidify the phenolic resin on the inner wall of the template structure, and further heating to decompose the template by heating and carbonize the phenolic resin to obtain the block material. Wherein, the xylem of the woody plant can be used as the template after being dried, and the method has the advantages of simple and easily obtained raw materials and simple preparation. |