http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108997238-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07D249-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B25-34 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07D249-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B25-34 |
filingDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108997238-B |
titleOfInvention | Preparation method of fine particle NTO |
abstract | The invention belongs to the technical field of energetic materials, and particularly relates to a preparation method of fine particle NTO. The invention provides a preparation method of fine particle NTO, which comprises the following steps: dropwise adding a dissolving solution of the raw material NTO into cold water under the stirring condition, and sequentially filtering and drying the mixed material liquid to obtain fine particle NTO; the solvent of the dissolving solution is nitrogen methyl pyrrolidone; the temperature of the dissolving solution is 60-80 ℃; the temperature of the cold water is 0-5 ℃; the stirring speed is 300-500 r/min. The preparation method provided by the invention has simple process, and the prepared NTO particles are finer and have narrower particle size distribution range. |
priorityDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |