classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-52
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-30
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-52
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30
filingDate 2018-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2021-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2021-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-108993492-B
titleOfInvention Preparation method of nanocatalyst with controllable morphology for decomposing methyl orange
abstract The invention provides a preparation method of a nano-catalyst with controllable shape for decomposing methyl orange, comprising the following steps: weighing metal according to chemical formula Al 100-a-b-c-d Ag a Ti b Pt c Aud Al, Ag, Ti, Pt and Au; smelting the metal into alloy ingots; placing the alloy ingots in the crucible of the gas atomization device, adding graphite particles to the crucible, and performing gas atomization to obtain mixed alloy powder; the mixed alloy The powder is sieved, and the graphite particles are sieved to obtain the alloy powder; the alloy powder is subjected to high-energy ball milling and the first heat treatment is performed; a sufficient amount of sodium hydroxide solution is poured into the amorphous alloy powder after the first heat treatment, and The alkali-treated alloy powder is filtered, and the filtered alloy powder is calcined to obtain a catalyst powder; and the catalyst powder is ball-milled for the second time. The preparation method of the invention does not involve complicated chemical reactions, is simple and easy to implement, has high yield and good catalytic effect.
priorityDate 2018-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419583196
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID104727
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23673835
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID409060395
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14798
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID407275646

Total number of triples: 27.