http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108927201-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 |
filingDate | 2018-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108927201-B |
titleOfInvention | A kind of preparation method and application of AgBr/g-C3N4 composite powder |
abstract | The invention discloses a preparation method and application of AgBr/g-C 3 N 4 composite powder, and relates to the technical field of composite powder preparation. Weigh cyanuric chloride, melamine and urea into a beaker, measure the acetonitrile reagent and pour it into the beaker, and stir it with a glass rod to disperse it; after stirring, pour the mixture into the reaction kettle, cover the reaction kettle and put it in. The reaction is carried out in a constant temperature blast oven; after the reaction is completed, the generated material is packed into a plastic test tube and centrifuged, washed and dried to obtain rod-shaped or tubular g-C 3 N 4 ; weigh g-C 3 N 4 , silver nitrate, CTAB Put it in a beaker, add absolute ethanol; pour the beaker into a plastic test tube after ultrasonic reaction, centrifuge, wash and dry to obtain AgBr/g-C 3 N 4 composite powder. The composite powder has a large specific surface area, a pore volume of 0.110cc/g, and a pore radius of 17.171nm; the composite powder has an excellent ability to degrade common organic dyes under visible light. |