abstract |
The invention discloses a preparation method of a ceramic grinding aid, and belongs to the technical field of ceramic treatment agents. Weighing 50-60 parts of solvent, 20-30 parts of additive, 5-8 parts of surfactant, 10-12 parts of modified soybean oil, 2-3 parts of water-soluble carbodiimide, 10-15 parts of microgel and 3-6 parts of water reducer in sequence according to parts by weight; mixing the microgel and a solvent in a stirrer, sequentially adding an additive, a surfactant, water-soluble carbodiimide, a water reducing agent and modified soybean oil into the stirrer, and stirring and mixing for 40-60 min at the temperature of 30-45 ℃ and the rotating speed of 300-500 r/min to obtain the ceramic grinding aid. |