http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108786796-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cc4e13141d402ceb885f368dfa042348 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-0033 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-10 |
filingDate | 2018-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa9376befb7d7aa6add03831472ef8c6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01bf7e7a25e9c68fd2338132fd095b26 |
publicationDate | 2018-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108786796-A |
titleOfInvention | A kind of PtAuPd@Ag core-shell structure copolymer nanocrystal elctro-catalysts and preparation method thereof |
abstract | The invention belongs to electrocatalysis material field, a kind of PtAuPd@Ag core-shell structure copolymer nanocrystal elctro-catalysts and preparation method thereof are disclosed.CTAB and glucose are dissolved in silver ammino solution and obtain precursor solution, reacts, is cooled to room temperature at 80~180 DEG C, supernatant is taken after the centrifugation of gained reaction solution, obtains Ag seed solutions;PVP and citric acid are dissolved in water, Ag seed solutions are then added, 60~120 DEG C are warming up to after stirring and evenly mixing, chloroplatinic acid, 2~8h of gold chloride and chlorine palladium acid insulation reaction is added;Gained reaction solution is washed, centrifuges to get PtAuPd@Ag core-shell structure copolymer nanocrystal elctro-catalysts.The preparation method simple process of the present invention, raw material are easy to get, and gained PtAuPd@Ag core-shell structure copolymers nanocrystal sizes and pattern are uniform, can be used for catalyzing glycerol electroxidation and prepare high added value product. |
priorityDate | 2018-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |