http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108671951-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 |
filingDate | 2018-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108671951-B |
titleOfInvention | Carbon nitride composite photocatalyst and preparation method and application thereof |
abstract | The invention discloses a carbon nitride composite photocatalyst and a preparation method and application thereof, wherein the preparation method comprises the following steps: (1) c 3 N 4 The powder is placed in ethanol solution for ultrasonic treatment to obtain milky C 3 N 4 Stripping liquid; (2) adding Bi (NO) 3 ) 3 .5H 2 O powder and AgNO 3 Powder is placed in the C 3 N 4 Stirring the ultrasonic stripping solution in a shading environment to obtain a mixed solution; (3) mixing Na 3 VO 4 Dropwise adding the solution into the mixed solution prepared in the step (2), stirring, centrifuging, drying and grinding to obtain BiVO 4 /Ag 3 VO 4 /C 3 N 4 . In the preparation of BiVO 4 /Ag 3 VO 4 In-process synchronization of introducing C 3 N 4 On the basis, in order to further widen the visible light responsiveness, the ultrasonic stripping C is selected 3 N 4 Preparation of BiVO from stripping solution 4 /Ag 3 VO 4 /C 3 N 4 A ternary heterojunction. |