http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108642869-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2200-25 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-3562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M11-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-61 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-356 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M23-00 |
filingDate | 2018-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108642869-B |
titleOfInvention | Preparation method of super-hydrophobic anti-ultraviolet fabric |
abstract | The invention discloses a preparation method of a super-hydrophobic anti-ultraviolet fabric. The method comprises the following steps: firstly, synthesizing an anti-ultraviolet compound of 1, 2-epoxypropyl ether aromatic ketone, and then modifying silicon dioxide to ensure that the anti-ultraviolet compound is grafted to the surface of silicon dioxide particles to endow the silicon dioxide with anti-ultraviolet capability; then sequentially immersing the fabric into a polyelectrolyte compound aqueous solution and a silicon dioxide aqueous dispersion, and enabling silicon dioxide particles to be adsorbed on the surface of the fabric through an electrostatic self-assembly method, so that the fabric is endowed with anti-ultraviolet performance and a rough surface required by super-hydrophobicity is constructed; finally, the fabric is further treated by the fluorine-free water repellent agent to obtain the super-hydrophobic performance. The fabric obtained by the invention has excellent uvioresistant performance and hydrophobicity, and the preparation method is simple and convenient. |