http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108623782-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7614 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-67 |
filingDate | 2017-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108623782-B |
titleOfInvention | Self-extinction light-cured resin, preparation method and application thereof |
abstract | The invention relates to a self-extinction light-cured resin, a preparation method and application thereof, wherein the self-extinction light-cured resin comprises modified TDI isocyanurate and modified TDI; under the condition of not adding a flatting agent, the light-cured resin has good flatting property; the raw materials for preparing the self-extinction light-cured resin comprise TDI monomer, monohydroxy acrylate compound, antioxidant, catalyst, terminator, polymerization inhibitor and optional diluent. The preparation method of the light-cured resin is simple and easy to implement, the light-cured resin is used for preparing the UV coating, no flatting agent is added into the UV coating, the pencil hardness of a paint film is more than 4H, and when the incident angle is 60 degrees, the glossiness is not higher than 30. |