http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108478450-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a94c68b707d5c8cd8309884102190262 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K8-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61Q19-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-25 |
filingDate | 2018-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3f816cff58a79ea2cd54c46232034e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f68b3144ec8565d2f6afc90c6009fc5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7596cbcbe1093c69c547f0fb9df3f8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58397fb897b4d0affe2e4b39782bfabf |
publicationDate | 2018-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108478450-A |
titleOfInvention | A kind of manufacturing method of Cosmetic Manufacture high-silicon quartzite powder |
abstract | The invention discloses a kind of manufacturing methods of Cosmetic Manufacture high-silicon quartzite powder, include the following steps:S1:Choose good quartz mineral aggregate;S2:It is machined to compared with small building stones by knocking stone, small building stones are rolled into sand grains by stone again, constantly add water, water to be flowed into sedimentation basin with sand grains in roller compaction process, the yellowish-brown epidermis on raw ore surface is removed;S3:Sand grains in sedimentation basin is transported into hothouse baking into dry sand grain, is then sieved using vibrating screen, iron is removed using bar magnet and row's magnet in screening process;S4:Dry sand grain after screening is placed in 700~900 DEG C of high temperature sintering furnace, 2~4h of high temperature sintering obtains sinter;S5:Sinter, dimethicone and iron oxide are added sequentially in colloid mill, 20~40min is fully refined.Preparation method of the present invention is simple, at low cost, small to the irritation of skin under the premise of ensureing that high-silicon quartzite powder white color is bright, is suitable for Cosmetic Manufacture. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113831113-A |
priorityDate | 2018-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.