abstract |
The invention provides a laminated film which is restrained from curling and easy to position a die during molding. The laminated film is composed of a laminate of at least a support and a resin layer formed from a resin, wherein an absolute value | B-A | of a difference between a spectral intensity ratio A, which is a spectral intensity ratio obtained by dividing a spectral intensity of a crystalline portion of the resin measured in one direction of the resin layer by a spectral intensity of an amorphous portion, and a spectral intensity ratio B, which is a spectral intensity ratio obtained by dividing a spectral intensity of a crystalline portion of the resin measured in the other direction orthogonal to the one direction of the resin layer by a spectral intensity of an amorphous portion, is in a range of 0.00 to 0.70. |