http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108431309-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2314-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2321-0211 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2500-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 |
filingDate | 2016-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108431309-B |
titleOfInvention | low creep fiber |
abstract | The present invention relates to a method for preparing gel-spun UHMWPE fibers, the method comprising the steps of: providing an intrinsic viscosity (IV) of at least 8 dl/g, a comonomer content (C BR ) of at least 0.05 SCB/1000TC, An ultra-high molecular weight polyethylene composition having a comonomer mass average distribution (C MAD ) of at least 0.05, wherein the comonomer has at least 4 carbon atoms; the composition is dissolved in a solvent to form a UHMWPE concentration of 2- 40 wt% polymer solution; spinning the polymer solution through a porous template to form solution fibers; cooling the solution fibers to below 80° C. to form gel fibers; drawing the fibers in at least one step to form drawn fibers; At least a portion of the solvent is removed before, during, or after stretching, wherein the ratio of C MAD to C BR is greater than 1.0. The present invention also relates to gel-spun UHMWPE fibers obtainable by this method and products comprising said gel-spun UHMWPE fibers. |
priorityDate | 2015-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 67.