abstract |
The present invention relates to a wastegate component for a turbocharger comprising an alloy comprising about 30 to about 42 wt % Ni, about 15 to about 28 wt % Cr, about 1 to about 5 wt % Cr, about 1 to about 4 wt. % Ti, and at least about 20 wt. % Fe, and to a method for making such a wastegate component. |