abstract |
The present invention provides a kind of expanded water-based polyurethane-modified acrylic acid woodware fireproof paint of facing, and raw material includes following components by weight:50 80 parts of woodwork coating resin, 20 30 parts of ammonium polyphosphate, 8 12 parts of melamine, 58 parts of pentaerythrite, 8 12 parts of titanium dioxide, 36 parts of dispersant, 0.1 0.3 parts of levelling agent, 0.1 0.3 parts of antifoaming agent, 24 parts of thickener, 0.1 0.3 parts of preservative, 1.0 2.5 parts of coalescents, 0.1 0.3 parts of wetting agent, 0.2 0.5 parts of 10 emulsifiers of OP, 30 50 parts of deionized water. |