http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108381711-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cbb14ed56c67e88afb089965c3d8c898 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-06 |
filingDate | 2018-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01fb80efdd3df2ac884c0ff8961e4683 |
publicationDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108381711-A |
titleOfInvention | A kind of timber sofening treatment method |
abstract | The invention discloses a kind of timber sofening treatment methods, include the following steps:Cutting, acidification, depickling processing, softening agent immersion, temperature-variable drying.Timber is first acidified by the present invention, depickling is handled, and acid-base neutralization can increase space between cells, so that it is more preferable to softening agent assimilation effect, then passes through temperature-variable drying and handle, promote the infiltration of softening agent, bating effect is more preferable, also avoids leading to the problem of dehydration suddenly and causes timber hard crisp. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113815073-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109571148-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109571148-B |
priorityDate | 2018-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 34.