http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108373175-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-485 |
filingDate | 2018-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108373175-B |
titleOfInvention | Aluminum-doped cobalt tetroxide, preparation method and application thereof |
abstract | The invention discloses a preparation method of aluminum doped cobalt tetroxide, comprising the following steps: (1) mixing an aluminum salt solution with a complexing agent to obtain a mixed solution; (2) mixing a cobalt salt solution and a carbonate ion-containing precipitant solution and the mixed solution prepared in step (1) is added to the reaction device in a co-current manner, and co-precipitated to obtain aluminum-doped cobalt carbonate; (3) the aluminum-doped cobalt carbonate prepared in step (2) is calcined, namely Aluminum-doped cobalt tetroxide can be obtained. The three solutions are fed in a co-current manner, which overcomes the problem of large differences in the sedimentation velocity of various elements in the process of preparing aluminum-doped cobalt tetroxide by a liquid-phase co-precipitation method. The prepared aluminum-doped tricobalt tetroxide has uniform distribution of each element, and the doping amount of the aluminum element in the aluminum-doped tricobalt tetroxide is significantly increased, and the doping amount is 0.3-0.6 percent. |