http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108329656-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2237 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate | 2018-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108329656-B |
titleOfInvention | High-toughness solid buoyancy material containing elastic microspheres and preparation method thereof |
abstract | The high-toughness solid buoyancy material containing elastic microspheres is prepared from 100 parts by mass of epoxy resin, 0-20 parts by mass of reactive diluent, 60-120 parts by mass of curing agent, 0-1 part by mass of accelerator, 0-20 parts by mass of toughening agent and 10-100 parts by mass of elastic microspheres. The elastic microspheres coated with the inorganic shell are used as the filler of the solid buoyancy material, so that the toughness of the final product is greatly improved, and the pressure resistance and the heat resistance of the final product are improved to a certain extent; meanwhile, after the surface modifier is added, the surface modification can be simultaneously carried out on the matrix resin and the elastic microspheres, so that the binding force between the inorganic matter shell on the surfaces of the elastic microspheres and the epoxy resin matrix is improved, and the overall toughness of the solid buoyancy material is improved. |
priorityDate | 2018-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links