abstract |
The composition for a non-aqueous secondary battery adhesive layer of the present invention contains organic particles and a water-soluble polymer, and the 1 mass % aqueous solution viscosity of the water-soluble polymer is 500 mPa·s or more and 9000 mPa·s or less, and the shear rate is The viscosity η 0 at 100 sec -1 is 10 mPa·s or more and 200 mPa·s or less, and the ratio of η 0 to the viscosity η 1 when the shear rate is 10000 sec- 1 is 1.5 or more and 5.0 or less. |