http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108264275-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b2eccf4a0ea6798c250fa0ddf5978303 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-00 |
filingDate | 2016-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6dc80919d1c5ab372f5f05fd292d4b4c |
publicationDate | 2018-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108264275-A |
titleOfInvention | A kind of dry-mixed mortar with cellulose |
abstract | The present invention relates to a kind of dry-mixed mortar with cellulose, component and part is:230 300 parts of iron ore mining and mill run clast, 60 130 parts of flyash, 120 200 parts of cement, 450 510 parts of middle sand, 47 parts of wood fibre, 59 parts of PP fibers, 11 16 parts of gypsum, 48 parts of latex powder, 37 parts of calcium nitrite, 15 parts of perlite;The present invention builds type premixing mortar by laying bricks or stones, and tensile strength is big, and cohesive force is strong, it is not easy to dry shrinkage and cracking;It is of low cost, trade waste is widely applied, product cost is not only reduced and can turn waste into wealth. |
priorityDate | 2016-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 17.